[* black] Sand the guitar using water-soaked sandpaper. | |
+ | [* black] Start with 600 grit sandpaper, follow it with 800 grit, then 1000 grit, then 1200 grit and finally 2000 grit. |
[* icon_note] When you feel less resistance while sanding, it is time to move on to a higher grit sandpaper or finish sanding. | |
- | [* icon_note] Start with 600 grit sandpaper, follow it with 800 grit, then 1000 grit, then 1200 grit and finally 2000 grit. |